摘要:
AbstractTechniques and equipment were developed for the extrusion of vapour deposited RAE Alloy 72. The alloy was extruded at temperatures from 300 to 420°C and extrusion ratios from 2:1 to 25:1. Room and elevated temperature strengths and smooth S–N (stress–number of cycles to failure) fatigue properties were determined for a range of extrusions. The best extrusions gave room and elevated temperature strengths that were comparable to those of rapidly solidified aluminium alloys. The fatigue strength/tensile strength ratio of>0·5 was higher than would be expected for an aluminium alloy.MST/1350