The thermoelectric figure of merit of silver selenide powders prepared by a low‐temperature process is examined. By careful attention to the process variables including the compaction, sintering temperature, and cooling rate through the &bgr;2phase it is possible to obtain ann‐type thermoelement having a figure of merit of 3×10−3per degree at room temperature.